本文二维码信息
二维码(扫一下试试看!)
不同种类研磨淀粉用于纸质食品包装的防油性能研究
Study on Oil Resistance of Different Kinds of Grinding Starch Used in Paper Food Packaging
投稿时间:2024-09-14  
DOI:10.11980/j.issn.0254-508X.2025.01.008
关键词:  食品包装  研磨淀粉  防油等级  吸油值  油接触角
Key Words:food packaging  grinding starch  oil resistance level  oil absorption value  oil contact angle
基金项目:
作者单位邮编
张瑞娟 中国制浆造纸研究院有限公司北京100102
制浆造纸国家工程实验室北京 100102 
100102
苏艳群 中国制浆造纸研究院有限公司北京100102
制浆造纸国家工程实验室北京 100102 
100102
夏菲 中国制浆造纸研究院有限公司北京100102
制浆造纸国家工程实验室北京 100102 
100102
刘金刚* 中国制浆造纸研究院有限公司北京100102
制浆造纸国家工程实验室北京 100102 
100102
肖贵华 中国制浆造纸研究院有限公司北京100102
制浆造纸国家工程实验室北京 100102
华南理工大学轻工科学与工程学院广东广州510640 
510640
孙德文 中国制浆造纸研究院有限公司北京100102
制浆造纸国家工程实验室北京 100102 
100102
杨小博 中国制浆造纸研究院有限公司北京100102
制浆造纸国家工程实验室北京 100102 
100102
黄举 中国制浆造纸研究院有限公司北京100102 100102
摘要点击次数: 99
全文下载次数: 29
摘要:本研究采用机械研磨法制备了超细淀粉分散液,用于对食品包装白卡纸进行涂布,以探讨淀粉的种类、研磨淀粉粒径及涂布量对白卡纸防油性能的影响。结果表明,研磨阳离子淀粉和研磨高交联淀粉M更有利于提高白卡纸防油性能。此外,淀粉研磨粒径越小、研磨淀粉涂布量越高,白卡纸的防油等级越高。以高交联淀粉M为原料,当淀粉研磨粒径为0.264 μm,涂布量为3.5 g/m2时,涂布白卡纸的透气度降低了98.0%,防油等级达6级,吸油值达0.87 g/m2,油接触角达93.2°;当涂布量从2.23 g/m2增加到6.20 g/m2,涂布白卡纸防油等级从2级增加至9级,透气度从0.059 3 μm·Pa·s下降到0.000 081 0 μm·Pa·s,吸油值从2.32 g/m2降低至0.59 g/m2
Abstract:Ultrafine grinding starch dispersion was prepared by mechanical progress and coated on the surface of white cardboard for food packaging. Then the effect of starch type, size of grinding starch and coating amount on oil resistance of white cardboard was studied. The results showed that grinding cationic starch and grinding highly crosslinked starch M were more beneficial to improve the oil resistance of white cardboard. In addition, the smaller the grinding starch particles size and the higher the coating amount, the higher the oil resistance level of white cardboard. Using highly crosslinked starch M as raw material with size of 0.264 μm, and the coating amount of 3.5 g/m2, the air permeability of coated white paperboard was reduced by 98.0%, the oil resistance level reached to 6, the oil absorption value reached to 0.87g/m2, and the oil contact angle reached to 93.2°. When the coating amount increased from 2.23 g/m2 to 6.20 g/m2, the oil resistance level of coated white paperboard increased from 2 to 9, and the air permeability decreased from 0.059 3 to 0.000 081 0 μm·Pa·s, the oil absorption decreased from 2.32 g/m2 to 0.59 g/m2.